    摘要:

    以软化点为85 ℃、0.30~0.45 mm的中温煤沥青颗粒为原料,采用悬浮法制备沥青球,采用混合氧化法(HNO3液相氧化和O2气相氧化)对沥青球进行不熔化处理. 不熔化沥青球经过炭化、CO2活化法制备沥青基球形活性炭. 采用SEM、TG/DTG、FT-IR对沥青球进行表征. 结果表明,采用悬浮法制备的沥青球表面光滑、平均球形度0.981、粒径分布集中,0.30~0.45 mm的沥青球质量占比超93%. 活化温度940 ℃,保温6 h制得的沥青基球形活性炭的BET比表面积为1 545 m2/g、微孔率为75.30%.

    Abstract:

    Using medium-temperature coal pitch particles with a softening point of 85 ℃ and a particle size of 0.30~0.45 mm as raw materials, pitch balls were prepared by the suspension method and stabilized by the mixed oxidation method(HNO3 oxidation and O2 oxidation). Pitch-based Spherical Activated Carbon is prepared from non-melting pitch balls through carbonization and CO2 activation. The pitch balls were characterized by SEM, TG/DTG, and FT-IR. The results show that the pitch balls prepared by the suspension method have a smooth surface, an average sphericity of 0.981, and a concentrated particle size distribution. The weight of the pitch ball of 0.30~0.45 mm accounts for more than 93%. After the activation temperature of 940 ℃ and 6 h of heat preservation, the BET specific surface area of Pitch-based Spherical Activated Carbon is 1 545.20 m2/g and the microporosity is 75.30%.

    参考文献
    相似文献
    引证文献
文章指标
  • PDF下载次数:
  • HTML阅读次数:
  • 摘要点击次数:
  • 引用次数:
引用本文

陈石林 ?,曾祥鸿 ,梁正 ,罗高强 ,梁玉林 ,宋振宇 .中温煤沥青悬浮法制备球形活性炭的研究[J].湖南大学学报:自然科学版,2022,49(12):115~121

复制
历史
  • 收稿日期:
  • 最后修改日期:
  • 录用日期:
  • 在线发布日期: 2023-01-02
  • 出版日期:
作者稿件一经被我刊录用,如无特别声明,即视作同意授予我刊论文整体的全部复制传播的权利,包括但不限于复制权、发行权、信息网络传播权、广播权、表演权、翻译权、汇编权、改编权等著作使用权转让给我刊,我刊有权根据工作需要,允许合作的数据库、新媒体平台及其他数字平台进行数字传播和国际传播等。特此声明。
关闭