    摘要:

    在有限元方法中利用动态模量主曲线和时间-温度位移因子来考虑荷载作用频率和温度对沥青混合料力学性质的影响,采用移动荷载模式,利用断裂力学的方法分析了典型柔性基层沥青路面的开裂机理.研究表明:轮载经过裂缝1次,根据不同工况,可能在裂尖引起1个,2个或3个张开型应力强度因子(KⅠ)峰值.而剪切型应力强度因子(KⅡ)总有2个峰值,且大小相等,方向相反.分析了温度、行车速度及裂缝长度对裂尖应力强度因子及其作用频率的影响.当裂缝较短且温度较低时,裂缝扩展主要由KⅠ引起.随着裂缝长度的增加和温度的升高,KⅡ逐渐成为裂缝扩展的主要因素.

    Abstract:

    In this study, the dynamic modulus master curves and time-temperature shift factors of asphalt mixtures were incorporated in finite element method to take into account the effects of the load frequency and temperature on the mechanical properties of asphalt mixtures. Bottom-up fatigue cracking of a typical asphalt pavement structure with flexible bases under moving load was analyzed with fracture mechanics. The results showed that one, two or three peaks of tensile type stress intensity factor ( KⅠ) at the crack tip could be induced during one passage of wheel load over the crack under various conditions, while two peaks of shear type stress intensity factor (KⅡ) always occurred,which were equal in magnitude but had opposite directions. The effects of temperature, vehicle speed and crack length on stress intensity factor and its frequency were analyzed. It was found that crack propagation was mainly controlled by KⅠ for pavements with short crack length and at low temperature, and KⅡ gradually became the main driving force for crack propagation as temperature and crack length increased.

    参考文献
    相似文献
    引证文献
文章指标
  • PDF下载次数:
  • HTML阅读次数:
  • 摘要点击次数:
  • 引用次数:
引用本文

赵延庆,王国忠,王志超,谭忆秋.基于动态模量的沥青路面开裂分析[J].湖南大学学报:自然科学版,2010,37(7):7~11

复制
历史
  • 收稿日期:
  • 最后修改日期:
  • 录用日期:
  • 在线发布日期:
  • 出版日期:
作者稿件一经被我刊录用,如无特别声明,即视作同意授予我刊论文整体的全部复制传播的权利,包括但不限于复制权、发行权、信息网络传播权、广播权、表演权、翻译权、汇编权、改编权等著作使用权转让给我刊,我刊有权根据工作需要,允许合作的数据库、新媒体平台及其他数字平台进行数字传播和国际传播等。特此声明。
关闭