+高级检索
聚氨酯多元醇水分散体的合成
DOI:
作者:
作者单位:

作者简介:

通讯作者:

基金项目:


Synthesis of Waterborne Polyurethane Polyol Dispersions
Author:
Affiliation:

Fund Project:

  • 摘要
  • |
  • 图/表
  • |
  • 访问统计
  • |
  • 参考文献
  • |
  • 相似文献
  • |
  • 引证文献
  • |
  • 资源附件
    摘要:

    以异佛尔酮二异氰酸酯(IPDI),聚醚二元醇(N210),二羟甲基丙酸(DMPA),三羟甲基丙烷(TMP)为主要原料制备端-NCO聚氨酯预聚体,用二乙醇胺(DEA)封端引入羟基,合成了双组分水性聚氨酯的聚氨酯多元醇分散体组分.研究发现:DMPA,TMP的用量、羟基含量及分散体与固化剂组分的配比等因素显著影响分散体及涂膜的性能.当DMPA质量分数为6%~6.5%,TMP质量分数为3%~5%,DEA质量分数为7.61%,-n-NCO ∶-n-OH 为1.5~1.7时,涂膜的光泽度、硬度、耐溶剂性、耐水性等最佳.采用傅立叶变换红外光谱、扫描电镜等仪器对多元醇合成过程和双组分水性聚氨酯涂膜进行了表征.

    Abstract:

    A polyurethane polyol dispersions of two-package waterborne polyurethane have been successfully synthesized with diethanolamine (DEA) as the blocking agent for introducing hydroxy-terminated on to the end-NCO polyurethane prepolymers, which were prepared beforehand with isophorone diisocyanate (IPDI), polyether binary alcohol (N210), dimethylol propionic acid (DMPA), and trimethylolpropane(TMP) as the main raw materials. The properties of the dispersions and films such as gloss, hardness, solvent resistance, water resistance were significantly affected by the amount of DMPA, TMP, hydroxy contents and the ratio of dispersions to curing agents. The optimum performance was obtained with the content of DMPA, TMP and DEA reaching 6%~6.5%, 3%~5% and 7.61% respectively, and the ratio of curing agents to dispersions being 1.5~1.7. Furthermore, the synthetic process of the polyol dispersions and the 2K-WPU films were characterized by multiple devices such as FTIR and SEM.

    参考文献
    相似文献
    引证文献
文章指标
  • PDF下载次数:
  • HTML阅读次数:
  • 摘要点击次数:
  • 引用次数:
引用本文

张旭东 ,胡军保,吴 娇,钱 帆,王 雪.聚氨酯多元醇水分散体的合成[J].湖南大学学报:自然科学版,2011,38(4):51~56