    摘要:

    以嵌贴CFRP-混凝土黏结的冻融耐久性为研究对象,通过拔出试验考察了冻融循环作用下嵌贴FRP与具有不同强度或抗冻性能混凝土的黏结性能,讨论了冻融循环下嵌贴FRP-混凝土界面黏结的退化机理;分析了冻融循环作用下混凝土槽至试件边缘距离、胶层厚度等因素对试件界面黏结性能的影响.试验结果表明:冻融循环作用下普通C30混凝土力学性能退化显著,添加引气防冻剂和减水剂的C30混凝土强度下降显著小于普通C30混凝土,C60混凝土强度反而有所提高;冻融循环导致了嵌贴CFRP-普通C30混凝土的黏结承载力下降和破坏模式转变,但嵌贴CFRP与抗冻混凝土间的黏结承载力没有显著降低,表明混凝土冻融损伤是冻融循环下嵌贴FRP-混凝土黏结退化的主要原因;槽壁厚度较小时,加载端槽壁混凝土出现锥形斜裂缝;胶层厚度较薄时,冻融循环作用下试件黏结承载力的降低较胶层较厚的试件更为显著.

    Abstract:

    The durability of the interface between NSM FRP and concrete under freeze-thawing cycles was examined. The pull-out tests were conducted to investigate the influence of freeze-thawing cycles on the bond performance between NSM FRP and concrete with normal strength, high strength, or additional frost resistance. The mechanism of the bond degradation between NSM FRP and concrete under the freeze-thawing cycles was also discussed. Moreover, the influences of the distance between concrete edge and groove (edge distance) and the thickness of epoxy adhesive on the bond durability of the NSM FRP were studied. The test results show that freeze-thawing cycling resulted in the strength deterioration of ordinary concrete, while the high strength concrete and the concrete with frost resistance showed no significant deterioration under freeze-thawing cycles. Freeze-thawing cycling also caused the transformation of failure mode and the relatively significant decrease in bond capacity for specimens using ordinary concrete. Nevertheless, it had no substantial impact on the bond performance of specimens made by concrete with high strength or frost resistance. This result indicates that the bond deterioration of NSM FRP under freeze-thawing cycles was caused by low strength of concrete. Moreover, the decrease of edge distance resulted in cone-shape cracks at the loading end. When the thickness of epoxy adhesive was reduced, the bond strength degradation induced by freeze-thawing cycles was more significant compared with that of specimens with thicker epoxy adhesive.

    参考文献
    相似文献
    引证文献
文章指标
  • PDF下载次数:
  • HTML阅读次数:
  • 摘要点击次数:
  • 引用次数:
引用本文

彭晖,刘洋,付俊俊,苏鹏,刘扬.冻融循环作用下表层嵌贴CFRP-混凝土界面黏结性能试验研究[J].湖南大学学报:自然科学版,2017,44(5):63~72

复制
历史
  • 收稿日期:
  • 最后修改日期:
  • 录用日期:
  • 在线发布日期: 2017-05-23
  • 出版日期:
作者稿件一经被我刊录用,如无特别声明,即视作同意授予我刊论文整体的全部复制传播的权利,包括但不限于复制权、发行权、信息网络传播权、广播权、表演权、翻译权、汇编权、改编权等著作使用权转让给我刊,我刊有权根据工作需要,允许合作的数据库、新媒体平台及其他数字平台进行数字传播和国际传播等。特此声明。
关闭