Research on High-density and High-strength Graphite Materials Prepared from Mesophase Microbeads Modified by Coal-tar Pitch
Author:
Affiliation:

Fund Project:

  • 摘要
  • |
  • 图/表
  • |
  • 访问统计
  • |
  • 参考文献
  • |
  • 相似文献
  • |
  • 引证文献
  • |
  • 资源附件
    摘要:

    为解决低粘结组分中间相炭微球(MCMB)自烧结性较差的问题,采用热分析和扫描电镜等表征方法,研究了煤沥青种类对改性MCMB粉体烧结性能及其所制备的石墨材料性能的影响.结果表明,采用溶液混合法可在MCMB粉体(D50=23 μm)表面均匀包覆一层煤沥青,并显著提高了低粘结组分MCMB粉体的烧结性能.以改性MCMB粉体为原料经等静压成型、焙烧和石墨化处理所制备的石墨材料均匀致密,抗折强度明显高于以未经改性处理的MCMB粉体为原料制备的石墨材料(22 MPa),并按改性用高温沥青、改质沥青和中温沥青的顺序依次升高,分别为27.7 MPa、42.7 MPa和56.9 MPa.

    Abstract:

    To deal with the problem of mesophase microbeads(MCMB) with a poor sinterability in less binder, thermal analysis and SEM were used to study the influence of different types of coal tar pitch on the sinterability of MCMB powder and performance of the graphite bulks. The results demonstrate that coal tar pitch can coat the surface of the MCMB(D50=23 μm) uniformly by dissolving the pitch and blending the mixture, so that the modified MCMB was obtained and the sinterability was improved. The graphite prepared from the modified MCMB was obtained by successive process of isostatic pressing, baking and graphitization, which had a dense and uniform micro-structure. And the flexural strength of the materials was obviously higher than those(22 MPa) made of unmodified MCMBs, and it increased to 27.7 MPa,42.7 MPa and 56.9 MPa,corresponding to the sequence of high softing pitch,modified pitch and middle softing pitch, respectively.

    参考文献
    相似文献
    引证文献
文章指标
  • PDF下载次数:
  • HTML阅读次数:
  • 摘要点击次数:
  • 引用次数:
引用本文

刘洪波,秦冬杰,陈惠,刘金平,杨程,侯冬冬.煤沥青改性中间相炭微球制备高密高强石墨的研究[J].湖南大学学报:自然科学版,2018,45(6):40~44

复制
历史
  • 收稿日期:
  • 最后修改日期:
  • 录用日期:
  • 在线发布日期: 2018-06-08
  • 出版日期:
作者稿件一经被我刊录用,如无特别声明,即视作同意授予我刊论文整体的全部复制传播的权利,包括但不限于复制权、发行权、信息网络传播权、广播权、表演权、翻译权、汇编权、改编权等著作使用权转让给我刊,我刊有权根据工作需要,允许合作的数据库、新媒体平台及其他数字平台进行数字传播和国际传播等。特此声明。
关闭