    摘要:

    为探明栓钉间距对钢-UHPC轻型组合桥面结构受力性能的影响规律,完成了3个钢-UHPC组合梁试件变幅疲劳试验,主要试验变量为栓钉间距(100 mm、150 mm、300 mm).在疲劳试验中,重点考察了栓钉间距对轻型组合桥面结构疲劳性能的影响,并关注了栓钉焊趾处钢面板受拉-短栓钉受剪耦合作用下的疲劳性能;而在疲劳后的剩余承载力试验中,探明了栓钉间距对疲劳后UHPC裂缝发展规律及抗弯承载力的影响.疲劳试验结果表明,当栓钉间距为300 mm时,单位荷载下的钢-UHPC界面滑移明显高于其他两个试件,但在疲劳加载过程中,界面滑移增长并不明显;对于U肋受压区底板应变,当栓钉间距为100 mm和150 mm时,整个疲劳试验过程无明显变化,而当栓钉间距为300 mm时,应变呈现微小的增大趋势;为分析试件中栓钉根部的钢面板拉-剪耦合疲劳受力状态,基于《公路钢混组合桥梁设计与施工规范》(JTG/T D64-01—2015)中的计算方法进行了分析,结果表明,该方法能够获得偏保守的计算结果.此外,疲劳后的剩余承载力试验表明,栓钉间距越小,试件的塑性变形能力越强,截面的抗弯承载力相应提高.分别按弹塑性理论和塑性理论计算了试件的剩余承载力,发现试件虽然经历了疲劳加载,但测承载力仍大于计算承载力,且基于塑性理论的计算结果更接近实测结果.

    Abstract:

    In order to reveal the influence law of the stud spacing on the behavior of steel-UHPC lightweight composite deck structures, variable amplitude fatigue tests were accomplished for three LWCD beam specimens and the stud spacing was chosen as the core parameter in the tests (i.e., 100 mm, 150 mm, 300 mm). In the fatigue tests, the influence of the stud spacing on the fatigue performance of the LWCD was revealed and the combined tension-shear fatigue properties of the steel deck plate at stud root positions were obtained. In the residual capacity test after the fatigue tests, the influence of stud spacing on the cracking evolution mechanism in UHPC and on the residual capacity of the specimens was captured. The fatigue tests indicated that when the stud spacing was 300 mm, the unit-load induced slips at the steel-UHPC interface were much higher than those in the other two specimens, but the slips did not increase significantly during the fatigue testing process. When the stud spacing was 100 mm or 150 mm, the strain at the bottom flange of the U rib did not exhibit significant change, and the strains increased slightly when the stud spacing was 300 mm. On the basis of the calculation method prescribed in the code of “Specifications for Design and Construction of Highway Steel-concrete Composite Bridge” in China, the combined tension-shear fatigue state of the steel deck plate at stud root positions was analyzed, and the results implied that this method could provide conservative results. In addition, the residual capacity test after the fatigue testing showed that the smaller the stud spacing, the smaller the interfacial slip and the higher the residual flexural capacity. On the basis of the elastic-to-plastic theory and plastic theory, the residual capacities of the specimens were predicted. It was revealed that although the specimens experienced a series of fatigue loading, the actual residual capacities obtained in the tests were still higher than the predicted values, and the plastic theory exhibits a better agreement relative to the test results.

    参考文献
    相似文献
    引证文献
文章指标
  • PDF下载次数:
  • HTML阅读次数:
  • 摘要点击次数:
  • 引用次数:
引用本文

曹君辉 ?,赵宇航 ,邵旭东 ,沈秀将 .钢-薄层UHPC轻型组合桥面结构抗弯疲劳及剩余承载力试验研究[J].湖南大学学报:自然科学版,2022,49(11):89~104

复制
历史
  • 收稿日期:
  • 最后修改日期:
  • 录用日期:
  • 在线发布日期: 2022-12-12
  • 出版日期:
作者稿件一经被我刊录用,如无特别声明,即视作同意授予我刊论文整体的全部复制传播的权利,包括但不限于复制权、发行权、信息网络传播权、广播权、表演权、翻译权、汇编权、改编权等著作使用权转让给我刊,我刊有权根据工作需要,允许合作的数据库、新媒体平台及其他数字平台进行数字传播和国际传播等。特此声明。
关闭