Abstract:The oxidation weight loss rate of binderless C/C composite prepared by in-situ carbonization of pre-oxidized fibres(PAN) was tested in the air,at 0.1 Mpa,from 673 K to 973 K using thermo-weight analysis method. The textures of this material before and aft