Abstract:Al-Cu-Co ternary alloy powders were fabricated with a new solid-liquid reaction milling technology. Al_(65)Co_(15)Cu_(20)powder was obtained by milling Al-33.2% Cu(mass friction)eutectic alloy melt at 923 K or 973 K for 12 hours, and Al_(69)Co_(